Our mission is usually to turn into an innovative provider of high-tech digital and communication devices by furnishing benefit added design and style, world-class manufacturing, and service capabilities for Zn Pellets , Gold Pellets , Vacuum Engineering , Created products with brand value. We attend seriously to produce and behave with integrity, and by the favor of customers at home and abroad in the xxx industry.
Factory wholesale Superalloy - Crti Alloy Sputtering Target High Purity Thin Film Pvd Coating Custom Made – Rich Detail:

The targets are prepared by mixing chromium and titanium powders or by vacuum melting and then compacting to full density. The material thus compacted can optionally be sintered and then formed into the desired target shape.

Chrome Titanium sputtering target has high purity, homogeneous microstructure, high density and low gas content. It is widely used in the formation of thin films for mold cutting tools. During the deposition process, a TiCN coating could be formed which could be applied directly to the exterior surface of a golf ball. TiCN coating could be closely attached onto metal surface. This kind of coating could perfectly fit the environment of Golf course for its excellent mechanical properties, toughness and hardness.

Our chromium titanium sputtering targets are carefully handled to prevent damage during storage and transportation and to preserve the quality of our products in their original condition.

Rich Special Materials specialises in the production of sputtering targets and can produce chromium and titanium sputtering materials to customer specifications. Our products have excellent mechanical properties, homogeneous structure, polished surfaces and no segregation, porosity or cracks. For more information, please contact us.


Product detail pictures:

Factory wholesale Superalloy - Crti Alloy Sputtering Target High Purity Thin Film Pvd Coating Custom Made – Rich detail pictures


Related Product Guide:

Our enhancement depends around the sophisticated devices ,exceptional talents and repeatedly strengthened technology forces for Factory wholesale Superalloy - Crti Alloy Sputtering Target High Purity Thin Film Pvd Coating Custom Made – Rich , The product will supply to all over the world, such as: Saudi Arabia, Birmingham, Greek, We now have to continue to uphold the "quality, detailed, efficient" business philosophy of "honest, responsible, innovative"spirit of service, abide by the contract and abide by reputation, first-class goods and improve service welcome overseas customers patrons.
  • In China, we have purchased many times, this time is the most successful and most satisfactory, a sincere and realiable Chinese manufacturer!
    5 Stars By Elsie from Qatar - 2018.10.09 19:07
    Wide range, good quality, reasonable prices and good service, advanced equipment, excellent talents and continuously strengthened technology forces,a nice business partner.
    5 Stars By Mona from Paraguay - 2017.02.18 15:54